Show simple item record

dc.contributor.authorKharchenko, V.V.
dc.contributor.authorStepanov, G.V.
dc.contributor.authorKravchenko, V.I.
dc.contributor.authorKobel'skii, S.V.
dc.contributor.authorBabutskyi, Anatolii
dc.contributor.authorTrunov , N.B.
dc.contributor.authorPiminov, V.A.
dc.date.accessioned2013-03-19T14:59:48Z
dc.date.available2013-03-19T14:59:48Z
dc.date.issued2009
dc.identifier.citationKharchenko , V V , Stepanov , G V , Kravchenko , V I , Kobel'skii , S V , Babutskyi , A , Trunov , N B & Piminov , V A 2009 , ' Redistribution of stresses in the header-PGV-1000 steam generator connector weldment under loading after thermal treatment ' , Strength of Materials , vol. 41 , no. 3 , pp. 251-256 . https://doi.org/10.1007/s11223-009-9130-7
dc.identifier.issn0039-2316
dc.identifier.otherPURE: 1056851
dc.identifier.otherPURE UUID: 97d68072-7a47-4619-97ab-51f026064515
dc.identifier.otherScopus: 67649414191
dc.identifier.urihttp://hdl.handle.net/2299/10189
dc.description.abstractAdditional heating of a thickened portion of the steam generator connector during postrepair thermal treatment of the header-connector weldment leads to a decrease in residual tensile stress levels. It is shown that during hydrostatic tests performed after thermal treatment inelastic strains on the inner connector surface are reduced, which inhances the cycle life of the weldmenten
dc.language.isoeng
dc.relation.ispartofStrength of Materials
dc.titleRedistribution of stresses in the header-PGV-1000 steam generator connector weldment under loading after thermal treatmenten
dc.contributor.institutionSchool of Engineering and Technology
dc.description.statusPeer reviewed
rioxxterms.versionofrecordhttps://doi.org/10.1007/s11223-009-9130-7
rioxxterms.typeJournal Article/Review
herts.preservation.rarelyaccessedtrue


Files in this item

FilesSizeFormatView

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record