Show simple item record

dc.contributor.authorD' Isanto, Fabiana
dc.contributor.authorSalvo, Milena
dc.contributor.authorMolin, Sebastian
dc.contributor.authorKoszelow, Damian
dc.contributor.authorJaved, Hassan
dc.contributor.authorAkram, Sufyan
dc.contributor.authorChrysanthou, Andreas
dc.contributor.authorSmeacetto, Federico
dc.date.accessioned2023-10-12T11:00:00Z
dc.date.available2023-10-12T11:00:00Z
dc.date.issued2022-10-01
dc.identifier.citationD' Isanto , F , Salvo , M , Molin , S , Koszelow , D , Javed , H , Akram , S , Chrysanthou , A & Smeacetto , F 2022 , ' Glass-ceramic joining of Fe22Cr porous alloy to Crofer22APU: interfacial issues and mechanical properties ' , Ceramics International , vol. 48 , no. 19, Part A , pp. 28519-28527 . https://doi.org/10.1016/j.ceramint.2022.06.166
dc.identifier.issn0272-8842
dc.identifier.otherORCID: /0000-0002-5708-2380/work/144393551
dc.identifier.urihttp://hdl.handle.net/2299/26905
dc.description© 2022 Elsevier Ltd and Techna Group S.r.l. All rights reserved. This is the accepted manuscript version of an article which has been published in final form at https://doi.org/10.1016/j.ceramint.2022.06.166
dc.description.abstractThis work deals with the joining of porous Fe22Cr ferritic stainless steel to a dense Crofer22APU plate by using a silica-based, Ba-containing glass-ceramic. The chemical and interfacial stability and the mechanical properties of the joints were evaluated before and after thermal ageing at 700°C for 500hrs. The sintering behaviour of the glass was assessed by using heating stage microscopy (HSM) to study the influence of a porous metal substrate on the shrinkage of the joining material. Scanning electron microscopy revealed that there were no defects or cracks at the porous alloy/glass-ceramic interface for both the as-joined samples and the samples after thermal ageing at 700°C for 500 hrs. However, at this exposure temperature, the porous alloy started to form an oxide scale at the interface with the glass-ceramic and the internal surface of the porous alloy. Finally, the evaluation of the mechanical properties by tensile testing showed that the properties were not affected by thermal ageing at 700°C.en
dc.format.extent9
dc.format.extent198947
dc.language.isoeng
dc.relation.ispartofCeramics International
dc.titleGlass-ceramic joining of Fe22Cr porous alloy to Crofer22APU: interfacial issues and mechanical propertiesen
dc.contributor.institutionDepartment of Engineering and Technology
dc.contributor.institutionECS Engineering and Technology VLs
dc.contributor.institutionSchool of Physics, Engineering & Computer Science
dc.contributor.institutionCentre for Future Societies Research
dc.contributor.institutionCentre for Climate Change Research (C3R)
dc.contributor.institutionMaterials and Structures
dc.contributor.institutionCentre for Engineering Research
dc.description.statusPeer reviewed
dc.date.embargoedUntil2024-06-16
rioxxterms.versionofrecord10.1016/j.ceramint.2022.06.166
rioxxterms.typeJournal Article/Review
herts.preservation.rarelyaccessedtrue


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record